POTASSIUM SODIUM ALLOY Eigenschaften

Schmelzpunkt:
6,8°C
Siedepunkt:
813°C
Dichte
0.87 g/mL at 25 °C
Dampfdruck
0 mm Hg ( 20 °C)
Aggregatzustand
liquid
Wichte
0.855
Sensitive 
air sensitive, moisture sensitive
EPA chemische Informationen
Potassium alloy, nonbase, K,Na (11135-81-2)
Sicherheit
  • Risiko- und Sicherheitserkl?rung
  • Gefahreninformationscode (GHS)
Kennzeichnung gef?hrlicher F,C
R-S?tze: 11-14/15-34-15
S-S?tze: 16-26-27-36/37/39-45-43
RIDADR  UN 1422 4.3/PG 1
WGK Germany  1
Selbstentzündungstemperatur 248-257 °F
HazardClass  4.3
PackingGroup  I
Bildanzeige (GHS) GHS hazard pictogramsGHS hazard pictograms
Alarmwort Achtung
Gefahrenhinweise
Code Gefahrenhinweise Gefahrenklasse Abteilung Alarmwort Symbol P-Code
H260 In Berührung mit Wasser entstehen entzündbare Gase, die sich spontan entzünden k?nnen. Stoffe und Gemische, die in Berührung mit Wasser entzündbare Gase entwickeln Kategorie 1 Achtung GHS hazard pictogramssrc="/GHS02.jpg" width="20" height="20" /> P223, P231+P232, P280, P335+ P334,P370+P378, P402+P404, P501
H314 Verursacht schwere Ver?tzungen der Haut und schwere Augensch?den. ?tzwirkung auf die Haut Kategorie 1B Achtung GHS hazard pictogramssrc="/GHS05.jpg" width="20" height="20" /> P260,P264, P280, P301+P330+ P331,P303+P361+P353, P363, P304+P340,P310, P321, P305+ P351+P338, P405,P501
Sicherheit
P223 Keinen Kontakt mit Wasser zulassen.
P231+P232 Unter inertem Gas handhaben. Vor Feuchtigkeit schützen.
P260 Dampf/Aerosol/Nebel nicht einatmen.
P280 Schutzhandschuhe/Schutzkleidung/Augenschutz tragen.
P303+P361+P353 BEI BERüHRUNG MIT DER HAUT (oder dem Haar): Alle kontaminierten Kleidungsstücke sofort ausziehen. Haut mit Wasser abwaschen oder duschen.
P305+P351+P338 BEI KONTAKT MIT DEN AUGEN: Einige Minuten lang behutsam mit Wasser spülen. Eventuell vorhandene Kontaktlinsen nach M?glichkeit entfernen. Weiter spülen.

POTASSIUM SODIUM ALLOY Chemische Eigenschaften,Einsatz,Produktion Methoden

R-S?tze Betriebsanweisung:

R11:Leichtentzündlich.
R14/15:Reagiert heftig mit Wasser unter Bildung hochentzündlicher Gase.
R34:Verursacht Ver?tzungen.
R15:Reagiert mit Wasser unter Bildung hochentzündlicher Gase.

S-S?tze Betriebsanweisung:

S16:Von Zündquellen fernhalten - Nicht rauchen.
S26:Bei Berührung mit den Augen sofort gründlich mit Wasser abspülen und Arzt konsultieren.
S27:Beschmutzte, getr?nkte Kleidung sofort ausziehen.
S36/37/39:Bei der Arbeit geeignete Schutzkleidung,Schutzhandschuhe und Schutzbrille/Gesichtsschutz tragen.
S45:Bei Unfall oder Unwohlsein sofort Arzt zuziehen (wenn m?glich, dieses Etikett vorzeigen).
S43:Zum L?schen . . . (vom Hersteller anzugeben) verwenden (wenn Wasser die Gefahr erh?ht, anfügen: "Kein Wasser verwenden").

Verwenden

Alternative to other reagents for desulfurizations, dehalogenations(as Wurtz coupling reactions), and Birch reductions.

Additionally can be used as:
  • A reducing agent for aliphatic ester substrates
  • A deprotectant in place of the typical heavy metal deprotectant

Sicherheitsprofil

A low-melting alloy of Na and K. Its toxicity is due to either Na or K alone. Corrosive to the eyes, skin, and mucous membranes. Upon contact with moisture it reacts violently to evolve H2; much heat; and a highly caustic residue of NaOH or KOH. Oxidation forms Na2O and K2O, whch are powerful caustics. A dangerous fire and explosion hazard. Violent or explosive reaction with O2, water, moisture, steam, halogens, oxidzers, acids or acid fumes, gving off much heat, hydrogen, toxic and corrosive fumes, often spattering either red-hot particles or actually flaming particles. A severe explosion hazard, wiU react explosively under the appropriate condtions with moisture, acids, acid fumes, solid CO2, carbon disulfide, halocarbons (e.g., CH3Cl, carbon tetrachloride, chloroform, bromoform,1,1,1- trichloroethane, 1,1,2- trichlorotrifluoroethane, tetrachloroethane, CH2Cl2, CH2l2), ammonium sulfate + NH4 + No3, HgO, metal halides (e.g., silver halides, zinc chloride, iron(Ⅲ) chloride), metal oxides (e.g., silver oxide, mercury oxide), nitrogen-containing explosives (e.g., ammonium nitrate, ammonium sulfate, picric acid, nitrobenzene), oxalyl bromide, oxalyl chloride, pentachloroethane, K oxides, KO2, Si, NaHCO3, polytetrafluoroethylene. Reacts vigorously with oxidizing materials. To fight fire, use G-1 powder, dry sodum chloride, dry sodium carbonate, dry calcium carbonate, dry sand, resin-coated sodium chloride, or dry soda ash. Never use water, graphite, carbon dioxide, halocarbons, or foam. Dangerous; when heated it emits highly toxic fumes of Na2O and K2O. Used as a liquid coolant for nuclear reactor cores. See also SODIUM and POTASSIUM.

POTASSIUM SODIUM ALLOY Upstream-Materialien And Downstream Produkte

Upstream-Materialien

Downstream Produkte


POTASSIUM SODIUM ALLOY Anbieter Lieferant Produzent Hersteller Vertrieb H?ndler.

Global( 26)Lieferanten
Firmenname Telefon E-Mail Land Produktkatalog Edge Rate
Hubei xin bonus chemical co. LTD
86-13657291602
linda@hubeijusheng.com CHINA 22963 58
Hebei Fengjia New Material Co., Ltd
+86-0311-87836622 +86-17333973358
sales06@hbduling.cn China 8054 58
Aladdin Scientific
+1-+1(833)-552-7181
sales@aladdinsci.com United States 57505 58
Meryer (Shanghai) Chemical Technology Co., Ltd. 021-61259108 18621169109
market03@meryer.com China 40228 62
Energy Chemical 021-021-58432009 400-005-6266
sales8178@energy-chemical.com China 44689 61
Shanghai Aladdin Bio-Chem Technology Co.,LTD 400-400-6206333 18521732826
market@aladdin-e.com China 25003 65
Sigma-Aldrich 021-61415566 800-8193336
orderCN@merckgroup.com China 51456 80
TCI (Shanghai) Chemical Trading Co., Ltd. 021-021-61109150
sales@tcisct.com China 31121 58
WUHAN JIXINYIBANG BIOTECHNOLOGY .,LTD 027-59768661 13297943853
1704244976@qq.com China 4272 58
Pand (Shanghai) international trade Co., LTD 18662931292 18662931292
3404730042@qq.com China 4759 58

11135-81-2()Verwandte Suche:


  • SODIUM-POTASSIUM ALLOY
  • POTASSIUM SODIUM ALLOY
  • Potassiumsodiumalloy78:22(99.95%)
  • potassiumsodiumalloys
  • sodiumpotassiumalloy,nak
  • SODIUM-POTASSIUM ALLOY (22% NA, 78% K)
  • SODIUM-POTASSIUM ALLOY (44% NA, 56% K)
  • Potassiumsodiumalloy78:22
  • Potassiumsodiumalloy56:44(99.95%)
  • Sodium potassium alloys
  • POTASSIUM SODIUM ALLOY, 3N5: 99.95%
  • POTASSIUM SODIUM ALLOY, 3N5
  • Alloy of potassium and sodium
  • Na2K-SG-I, Sodium-potassium alloy on silica gel (Na2K)
  • NaK Silica gel (Na2K) Stage I
  • K2Na-SG-I, Sodium-potassium alloy on silica gel (K2Na)
  • NaK Silica gel (K2Na) Stage I
  • potassium sodium alloy 56:44
  • NaK Silica gel (Na2K) Stage I extent of labeling: ~35 wt. % Na-K loading
  • NaK Silica gel (K
  • SodiuM-potassiuM alloy(SodiuM 44 wt. %, PotassiuM 56 wt. %)
  • Potassium alloy, nonbase, K,Na
  • 11135-81-2
  • Na2K
  • KNa
  • Alkali Metals
  • Synthetic Reagents
  • Reduction
  • Alkali MetalsMaterials Science
  • Alloys
  • Metal and Ceramic Science
  • Reduction
  • Synthetic Reagents
  • AlloysEssential Chemicals
  • Adsorbents, Filter Aids and Drying Agents
  • Other Drying Agents
Copyright 2019 ? ChemicalBook. All rights reserved